Secondary laboratory analysis of a randomised trial (10 participants): after six months' use, 3D-printed retainers were rougher than thermoformed ones and lost hardness and stiffness, while thermoformed retainers gained them. Small pilot sample.
Secondary analysisn = 10
Boo et al. A randomised controlled trial comparing thermoformed and 3D-printed retainers in young adults: evaluation of surface roughness, surface morphology, and mechanical properties